Category

Contact us

GSL-1100X-RC Superalloy High-Pressure Hydrothermal Reactor with 1100°C Max Temperature and 4 MPa Oxygen/Inert Gas Pressure

Designed for advanced material synthesis via hydrothermal methods under high oxygen pressure.
Constructed from Ni-based superalloy for excellent creep strength and oxidation resistance.
Operates up to 1100°C and 4 MPa pressure with real-time temperature and pressure monitoring.
Available in 65 mL and 100 mL vessel capacities with automatic pressure relief valve.

Compliance: CE Certified
Customized: OEM/ODM
Package: Plywood case package

Products

GSL-1100X-RC Superalloy High-Pressure Hydrothermal Reactor with 1100°C Max Temperature and 4 MPa Oxygen/Inert Gas Pressure

The GSL-1100X-RC reactor is engineered for hydrothermal synthesis and heat treatment of materials requiring elevated temperatures and controlled high-pressure oxygen or inert gas environments. Its Ni-based superalloy construction provides superior creep strength and oxidation resistance, enabling reliable operation at temperatures up to 1100°C and pressures up to 4 MPa. This makes it particularly suitable for preparing advanced materials and conducting experiments under aggressive oxidative conditions.

Equipped with a solenoid valve integrated into the flange, the reactor allows automatic pressure relief to maintain safe operating conditions. The system includes digital temperature control with 30 programmable segments and precision pressure sensors for real-time monitoring. Two vessel sizes are available—65 mL and 100 mL—each designed with an air-cooled flange and aluminum heat radiator to optimize thermal management.

Key Features

  • Pressure vessel made from Ni-based superalloy for high creep strength and oxidation resistance.
  • Maximum operating temperature of 1100°C and pressure up to 4 MPa under oxygen or inert gas.
  • Automatic pressure relief via solenoid valve installed on the flange for enhanced safety.
  • Digital temperature controller with 30-segment programmable heating and ±1°C accuracy.
  • Real-time temperature and pressure monitoring software included for precise process control.
  • Available vessel capacities: 65 mL (55 mm OD x 20 mm ID) and 100 mL (65 mm OD x 25 mm ID).
  • Omega K-type thermocouple with high-temperature tolerance and air-cooled flange design.

Technical Specifications

Parameter Specification
Pressure Vessel Material Ni-based Superalloy
Vessel Capacities and Dimensions 65 mL: 55 mm OD x 20 mm ID x 214 mm height; 100 mL: 65 mm OD x 25 mm ID x 210 mm height
Maximum Temperature 1100°C
Maximum Pressure 4 MPa at 1100°C (oxygen or inert gas)
Temperature Controller Digital, 30 programmable segments, ±1°C accuracy
Thermocouple Omega K-type, 3 mm OD, high-temperature connector (220°C tolerance)
Pressure Sensor Precision sensor with measurement range up to 250 bars
Pressure Relief Valve Solenoid valve with 15 MPa max relief pressure (manual needle valve for >15 MPa)
Power Supply AC 208–240 V, Single Phase, 2 kW

Typical Applications

This reactor is ideal for hydrothermal synthesis of advanced materials requiring high temperature and oxygen-rich or inert atmospheres. It is frequently used for heat treatment of samples under elevated oxygen pressure and can also function as a steam generator for specialized processes.

Configuration & Operating Notes

The reactor includes a SS316 needle valve with 1/4″ pipe connector and pressure gauge. Two copper gaskets (48 mm O.D.) are supplied as consumables. Optional accessories include torque wrenches to ensure proper flange bolt tightening and replacement liners made from various materials to suit different sample growth requirements.

For safety, the reactor and furnace must be operated inside an explosion-proof enclosure when under high pressure. Users must never face the top flange without protection. A two-stage pressure regulator should be installed on the gas supply to limit pressure below 3 PSI. Samples must be loaded in quartz or alumina boats; direct contact with the vessel is prohibited to avoid damage. Wrapping crucibles with gold or nickel foil is recommended to minimize contamination.