Category

Contact us

OTF1200XHP55 High Pressure Oxygen Tube Furnace with 20mm ID Ni-Based Superalloy Tube, Up to 1100°C at 610 PSI

Designed for high-pressure material processing under oxidizing and inert atmospheres.
Ideal for synthesizing new compounds and mini HIP treatment of metallic samples.
Features a Ni-based superalloy tube with 20 mm inner diameter and max temperature of 1100°C.
Operates safely up to 610 PSI (4.2 MPa) pressure with precise temperature and pressure control.

Compliance: CE Certified
Customized: OEM/ODM
Package: Plywood case package

Products

OTF1200XHP55 High Pressure Oxygen Tube Furnace with 20mm ID Ni-Based Superalloy Tube, Up to 1100°C at 610 PSI

The OTF1200XHP55 is engineered for advanced laboratory applications requiring controlled high-pressure and high-temperature environments. It is particularly suited for the synthesis and treatment of special compounds under oxygen and inert gas atmospheres, enabling researchers to prepare novel materials and perform mini hot isostatic pressing (HIP) on metallic samples.

This split tube furnace incorporates a nickel-based superalloy processing tube with a 20 mm internal diameter and 55 mm outer diameter, designed to withstand pressures up to 7 MPa (approximately 1015 PSI) and temperatures reaching 1100°C. The furnace features precise temperature control with a programmable PID system and integrated pressure monitoring with safety alarms and automatic pressure relief mechanisms.

Key Features

  • Ni-based superalloy tube (Waspaloy or equivalent) with 20 mm ID and 580 mm length for high-pressure operation.
  • Maximum operating temperature of 1100°C with heating rates up to 30°C/min.
  • Pressure capability up to 610 PSI (4.2 MPa) at 1100°C, with higher pressures allowed at lower temperatures.
  • Double-layer steel casing with air cooling and high-purity alumina insulation for energy efficiency.
  • Integrated precision pressure sensor and digital display with alarm and automatic pressure relief valve.
  • PC control via included laptop and pre-installed software for remote temperature and pressure monitoring.
  • Compatible with oxygen and inert gases (N2, Ar, He) and requires use of crucibles or isolated foil to protect the tube from sample contamination.

Technical Specifications

Parameter Specification
Model OTF1200XHP55
Processing Tube Material Ni-based superalloy (Waspaloy or equivalent)
Tube Dimensions (O.D x I.D x Length) 55 mm x 20 mm x 580 mm
Max Temperature 1100°C
Max Heating Rate ≤ 30°C/min
Continuous Heating Range Room Temperature to 1000°C
Heating Zone Length 250 mm (single zone)
Temperature Uniformity ±1°C over 50 mm zone, ±2°C over 70 mm zone
Power 2.5 kW
Voltage AC 208-240 V, Single Phase, 50/60 Hz
Pressure Range Up to 7 MPa (1015 PSI) max; operating limits vary with temperature
Pressure Sensor Range 0–25 MPa
Temperature Control MET certified 30 programmable segments, PID auto-tune, ±1°C accuracy
Thermocouple Omega 3 mm OD K-type
Heating Element Fe-Cr-Al alloy doped with Mo
Included Accessories Laptop with control software, superalloy flange, solenoid valve, pressure transmitter

Typical Applications

This furnace is used for high-pressure oxygen and inert gas treatments in material science research, including hydroretorting of shale oil, synthesis of advanced ceramics, and mini hot isostatic pressing of metals. It supports experiments requiring precise atmosphere control and elevated temperature and pressure conditions.

Configuration & Operating Notes

Samples must be loaded inside a quartz or alumina crucible or wrapped in isolated foil to prevent reaction with the Ni-based tube. Over-tightening flange bolts should be avoided; a torque wrench is recommended to apply the specified 40-foot pound torque. The furnace includes safety features such as pressure alarms and automatic pressure relief valves. Optional accessories include high-pressure electrical feedthroughs and sapphire windows for optical access.

Product Relate

MSK-HRP-3-E laboratory product view 1
MSK-HTML-LD laboratory product view 1
OTF-1200X-III-HVC-LD laboratory product view 2
KSL-1500X-GS125 laboratory product view 1
Scroll to Top