GSL-1100X-NI-1500 1.5L Ni-Based Superalloy High Pressure Reactor with 1000°C Max Temperature and 1 MPa Pressure for Hydrothermal and Steam Generation Applications

Designed for advanced material synthesis via hydrothermal methods and high oxygen pressure heat treatment.
Constructed from Ni-based superalloy for superior creep strength and oxidation resistance.
Operates up to 1000°C at 1 MPa with integrated pressure relief and remote monitoring software.

Compliance: CE Certified
Customized: OEM/ODM
Package: Plywood case package

Products

GSL-1100X-NI-1500 1.5L Ni-Based Superalloy High Pressure Reactor with 1000°C Max Temperature and 1 MPa Pressure for Hydrothermal and Steam Generation Applications

The GSL-1100X-NI-1500 reactor is engineered to facilitate high-temperature and high-pressure material processing, particularly suited for hydrothermal synthesis and heat treatment under elevated oxygen pressures. Its vertical furnace design incorporates a nickel-based superalloy chamber, providing excellent resistance to creep deformation and oxidation, essential for maintaining integrity at temperatures up to 1000°C and pressures reaching 1 MPa.

This reactor also functions effectively as a steam generator, expanding its utility in laboratory environments requiring controlled steam production. The system integrates a solenoid valve on the flange for automated pressure relief, enhancing operational safety. Additionally, included software enables precise temperature control and pressure monitoring remotely, facilitating user convenience and process accuracy.

Key Features

  • Ni-based superalloy GH747 reactor chamber with 1500 mL effective volume (112 mm OD x 100 mm ID x 280 mm height).
  • Capable of operating at pressures up to 3.5 MPa at 800°C, 2.0 MPa at 900°C, and 1.0 MPa at 1000°C.
  • Heating chamber dimensions: 120 mm ID x 200 mm height with Fe-Cr-Al alloy heating element and K-type thermocouple.
  • Dual digital temperature controllers with 30 programmable segments, ±1°C accuracy, and maximum continuous operation at 1000°C.
  • Integrated pressure sensor with high-pressure alarm and automatic pressure relief via solenoid valve.
  • Stainless steel outer casing with over-temperature and over-pressure safety interlocks.
  • Includes SS316 needle valve with pressure gauge and consumable copper gaskets.

Technical Specifications

Parameter Specification
Model GSL-1100X-NI-1500
Reactor Material Ni-based superalloy GH747
Effective Capacity 1500 mL
Reactor Dimensions (OD x ID x H) 112 mm x 100 mm x 280 mm
Heating Chamber Size (ID x H) 120 mm x 200 mm
Heating Element Fe-Cr-Al alloy
Thermocouple K-type, 3 mm OD with high-temp connector
Operating Pressure Limits 3.5 MPa ≤ 800°C; 2.0 MPa ≤ 900°C; 1.0 MPa ≤ 1000°C; 0.7 MPa ≤ 1100°C (1 hour max)
Max Continuous Temperature 1000°C
Max Temperature (Short Term) 1100°C (up to 1 hour)
Temperature Control Two digital controllers, 30 programmable segments, ±1°C accuracy
Power Supply 208-240 VAC, 50/60 Hz, single phase, 2.5 kW
Pressure Monitoring High-pressure sensor (up to 10 bar) with alarm and solenoid valve relief
Included Accessories SS316 needle valve with pressure gauge, two copper gaskets (63 mm OD)

Typical Applications

Ideal for hydrothermal synthesis of advanced materials, especially where high oxygen pressure and elevated temperatures are required. Suitable for heat treatment processes under controlled atmospheres and as a laboratory steam generator.

Configuration & Operating Notes

The reactor flange includes a solenoid valve for automatic pressure relief and a high-pressure alarm system. Users should avoid overtightening flange screws to prevent damage; torque wrench use is recommended. For safety, the high-pressure vessel must be operated inside an explosion-proof enclosure when under pressure. The recommended heating and cooling rates are 5 to 10°C per minute.