RC-NI500-V Ni-Based Superalloy High Pressure Hydrothermal Reactor
The RC-NI500-V reactor is engineered for precise hydrothermal synthesis and heat treatment of advanced materials under controlled high-pressure oxygen or inert atmospheres. Its construction from a nickel-based superalloy, such as Waspaloy or an equivalent, ensures exceptional creep strength and resistance to oxidation, enabling reliable operation at elevated temperatures up to 1100°C.
This reactor supports pressures up to 20 MPa at lower temperatures, with maximum allowable pressures decreasing as temperature rises, reaching 3 MPa at 1100°C. It is available in multiple capacities, including 300 mL and 500 mL volumes, accommodating various sample sizes and experimental requirements. The design includes a stainless steel 306 needle valve with a 1/4″ pipe connector for controlled gas flow.
Key Features
- Constructed from Ni-based superalloy (Waspaloy or equivalent) for high-temperature strength and oxidation resistance.
- Operating temperature range from room temperature up to 1100°C.
- Pressure capabilities vary with temperature: up to 20 MPa at 600°C, decreasing to 3 MPa at 1100°C.
- Available reactor volumes: 300 mL and 500 mL options to suit different experimental scales.
- Includes SS306 needle valve with 1/4″ pipe connector for precise gas regulation.
- Optional accessories include 304SS tube fittings, pressure relief valves, and digital pressure gauges.
- Compatible with vertical furnaces and temperature controllers for integrated heat treatment processes.
Technical Specifications
| Parameter | Specification |
|---|---|
| Material | Ni-Based Superalloy (Waspaloy or equivalent) |
| Reactor Capacity & Dimensions | 300 mL: 70 mm OD x 35 mm ID x 300 mm height; 500 mL: 70 mm OD x 35 mm ID x 500 mm height |
| Maximum Operating Temperature | 1100°C |
| Maximum Operating Pressure | 20 MPa at 600°C; 16.5 MPa at 800°C; 10 MPa at 900°C; 5 MPa at 1000°C; 3 MPa at 1100°C |
| Included Accessories | SS306 needle valve with 1/4″ pipe connector |
| Optional Accessories | 304SS 1/4″ O.D tube fittings, pressure relief valve, digital pressure gauge, vertical furnace with temperature controller |
Typical Applications
This reactor is ideal for hydrothermal synthesis of advanced materials requiring high temperature and oxygen or inert gas pressure conditions. It is particularly suited for sample heat treatment processes under elevated oxygen pressures, enabling controlled oxidation and phase formation studies.
Configuration & Operating Notes
For safe operation, the reactor and furnace must be housed inside an explosion-proof enclosure when under high pressure. Operators should avoid positioning themselves directly above the top flange during use. Installation of a gas pressure regulator is essential to control gas supply pressure and prevent overpressurization. Optional safety accessories such as pressure relief valves and digital gauges are recommended to enhance operational safety.